Extraction of flow behavior and hall–petch parameters using a nanoindentation multiple sharp tip approach

Research output: Contribution to journalArticleResearchpeer-review

Standard

Bibtex - Download

@article{3e1659b97af34e9895cf2afc69e565cc,
title = "Extraction of flow behavior and hall–petch parameters using a nanoindentation multiple sharp tip approach",
author = "Alexander Leitner and Verena Maier-Kiener and Daniel Kiener",
year = "2017",
doi = "10.1002/adem.201600669",
language = "English",
volume = "19",
journal = "Advanced Engineering Materials",
issn = "1527-2648",
publisher = "Wiley-VCH ",
number = "4",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Extraction of flow behavior and hall–petch parameters using a nanoindentation multiple sharp tip approach

AU - Leitner, Alexander

AU - Maier-Kiener, Verena

AU - Kiener, Daniel

PY - 2017

Y1 - 2017

U2 - 10.1002/adem.201600669

DO - 10.1002/adem.201600669

M3 - Article

VL - 19

JO - Advanced Engineering Materials

JF - Advanced Engineering Materials

SN - 1527-2648

IS - 4

M1 - 1600669

ER -