Extraction of flow behavior and hall–petch parameters using a nanoindentation multiple sharp tip approach
Research output: Contribution to journal › Article › Research › peer-review
Authors
Organisational units
Details
Original language | English |
---|---|
Article number | 1600669 |
Number of pages | 9 |
Journal | Advanced Engineering Materials |
Volume | 19 |
Issue number | 4 |
DOIs | |