Interaction of the precipitation kinetics of δ and γ' phases in nickel-base superalloy ATI Allvac® 718Plus™

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Standard

Interaction of the precipitation kinetics of δ and γ' phases in nickel-base superalloy ATI Allvac® 718Plus™. / Radis, Rene; Zickler, Gerald A.; Stockinger, Martin et al.
THERMEC 2009. ed. / Tara Chandra; Tara Chandra; Tara Chandra; N. Wanderka; N. Wanderka; N. Wanderka; Walter Reimers; Walter Reimers; Walter Reimers; M. Ionescu; M. Ionescu; M. Ionescu. 2010. p. 2712-2717 (Materials Science Forum; Vol. 638-642).

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Harvard

Radis, R, Zickler, GA, Stockinger, M, Sommitsch, C & Kozeschnik, E 2010, Interaction of the precipitation kinetics of δ and γ' phases in nickel-base superalloy ATI Allvac® 718Plus™. in T Chandra, T Chandra, T Chandra, N Wanderka, N Wanderka, N Wanderka, W Reimers, W Reimers, W Reimers, M Ionescu, M Ionescu & M Ionescu (eds), THERMEC 2009. Materials Science Forum, vol. 638-642, pp. 2712-2717, 6th International Conference on Processing and Manufacturing of Advanced Materials - THERMEC'2009, Berlin, Germany, 25/08/09. https://doi.org/10.4028/www.scientific.net/MSF.638-642.2712

APA

Radis, R., Zickler, G. A., Stockinger, M., Sommitsch, C., & Kozeschnik, E. (2010). Interaction of the precipitation kinetics of δ and γ' phases in nickel-base superalloy ATI Allvac® 718Plus™. In T. Chandra, T. Chandra, T. Chandra, N. Wanderka, N. Wanderka, N. Wanderka, W. Reimers, W. Reimers, W. Reimers, M. Ionescu, M. Ionescu, & M. Ionescu (Eds.), THERMEC 2009 (pp. 2712-2717). (Materials Science Forum; Vol. 638-642). https://doi.org/10.4028/www.scientific.net/MSF.638-642.2712

Vancouver

Radis R, Zickler GA, Stockinger M, Sommitsch C, Kozeschnik E. Interaction of the precipitation kinetics of δ and γ' phases in nickel-base superalloy ATI Allvac® 718Plus™. In Chandra T, Chandra T, Chandra T, Wanderka N, Wanderka N, Wanderka N, Reimers W, Reimers W, Reimers W, Ionescu M, Ionescu M, Ionescu M, editors, THERMEC 2009. 2010. p. 2712-2717. (Materials Science Forum). doi: 10.4028/www.scientific.net/MSF.638-642.2712

Author

Radis, Rene ; Zickler, Gerald A. ; Stockinger, Martin et al. / Interaction of the precipitation kinetics of δ and γ' phases in nickel-base superalloy ATI Allvac® 718Plus™. THERMEC 2009. editor / Tara Chandra ; Tara Chandra ; Tara Chandra ; N. Wanderka ; N. Wanderka ; N. Wanderka ; Walter Reimers ; Walter Reimers ; Walter Reimers ; M. Ionescu ; M. Ionescu ; M. Ionescu. 2010. pp. 2712-2717 (Materials Science Forum).

Bibtex - Download

@inproceedings{2bb2732b6fef4beb97260be08dc4c39a,
title = "Interaction of the precipitation kinetics of δ and γ' phases in nickel-base superalloy ATI Allvac{\textregistered} 718Plus{\texttrademark}",
keywords = "ATI Allvac{\textregistered} 718Plus{\texttrademark}, Delta, Gamma prime, Precipitation kinetics, Superalloy",
author = "Rene Radis and Zickler, {Gerald A.} and Martin Stockinger and Christof Sommitsch and Ernst Kozeschnik",
year = "2010",
doi = "10.4028/www.scientific.net/MSF.638-642.2712",
language = "English",
isbn = "0878492941",
series = "Materials Science Forum",
pages = "2712--2717",
editor = "Tara Chandra and Tara Chandra and Tara Chandra and N. Wanderka and N. Wanderka and N. Wanderka and Walter Reimers and Walter Reimers and Walter Reimers and M. Ionescu and M. Ionescu and M. Ionescu",
booktitle = "THERMEC 2009",
note = "6th International Conference on Processing and Manufacturing of Advanced Materials - THERMEC'2009 ; Conference date: 25-08-2009 Through 29-08-2009",

}

RIS (suitable for import to EndNote) - Download

TY - GEN

T1 - Interaction of the precipitation kinetics of δ and γ' phases in nickel-base superalloy ATI Allvac® 718Plus™

AU - Radis, Rene

AU - Zickler, Gerald A.

AU - Stockinger, Martin

AU - Sommitsch, Christof

AU - Kozeschnik, Ernst

PY - 2010

Y1 - 2010

KW - ATI Allvac® 718Plus™

KW - Delta

KW - Gamma prime

KW - Precipitation kinetics

KW - Superalloy

UR - http://www.scopus.com/inward/record.url?scp=75849154501&partnerID=8YFLogxK

U2 - 10.4028/www.scientific.net/MSF.638-642.2712

DO - 10.4028/www.scientific.net/MSF.638-642.2712

M3 - Conference contribution

AN - SCOPUS:75849154501

SN - 0878492941

SN - 9780878492947

T3 - Materials Science Forum

SP - 2712

EP - 2717

BT - THERMEC 2009

A2 - Chandra, Tara

A2 - Chandra, Tara

A2 - Chandra, Tara

A2 - Wanderka, N.

A2 - Wanderka, N.

A2 - Wanderka, N.

A2 - Reimers, Walter

A2 - Reimers, Walter

A2 - Reimers, Walter

A2 - Ionescu, M.

A2 - Ionescu, M.

A2 - Ionescu, M.

T2 - 6th International Conference on Processing and Manufacturing of Advanced Materials - THERMEC'2009

Y2 - 25 August 2009 through 29 August 2009

ER -