Studies on the melting behavior of polypropylene nano-composites using X-ray diffraction and differential scanning calorimetry

Publikationen: Beitrag in Buch/Bericht/KonferenzbandBeitrag in Konferenzband

Standard

Studies on the melting behavior of polypropylene nano-composites using X-ray diffraction and differential scanning calorimetry. / Feuchter, Michael; Maier, Günther; Pinter, Gerald et al.
ANTEC 2009 Society of Plastics Engineers' Annual Technical Conference. 2009. S. 2642-2646.

Publikationen: Beitrag in Buch/Bericht/KonferenzbandBeitrag in Konferenzband

Author

Feuchter, Michael ; Maier, Günther ; Pinter, Gerald et al. / Studies on the melting behavior of polypropylene nano-composites using X-ray diffraction and differential scanning calorimetry. ANTEC 2009 Society of Plastics Engineers' Annual Technical Conference. 2009. S. 2642-2646

Bibtex - Download

@inproceedings{8dc7898952ff48be9ba7374d18682ba4,
title = "Studies on the melting behavior of polypropylene nano-composites using X-ray diffraction and differential scanning calorimetry",
author = "Michael Feuchter and G{\"u}nther Maier and Gerald Pinter and Milan Kracalik and Stephan Laske and G{\"u}nter Langecker",
year = "2009",
language = "English",
pages = "2642--2646",
booktitle = "ANTEC 2009 Society of Plastics Engineers' Annual Technical Conference",

}

RIS (suitable for import to EndNote) - Download

TY - GEN

T1 - Studies on the melting behavior of polypropylene nano-composites using X-ray diffraction and differential scanning calorimetry

AU - Feuchter, Michael

AU - Maier, Günther

AU - Pinter, Gerald

AU - Kracalik, Milan

AU - Laske, Stephan

AU - Langecker, Günter

PY - 2009

Y1 - 2009

M3 - Conference contribution

SP - 2642

EP - 2646

BT - ANTEC 2009 Society of Plastics Engineers' Annual Technical Conference

ER -