Nanoindentation and wear properties of Ti and Ti-TiB composite materials produced by selective laser melting
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Standard
in: Materials science and engineering: A, Structural materials: properties, microstructure and processing, Jahrgang 688, 03.2017, S. 20-26.
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Harvard
APA
Vancouver
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Nanoindentation and wear properties of Ti and Ti-TiB composite materials produced by selective laser melting
AU - Attar, Hooyar
AU - Ehtemam-Haghighi, S.
AU - Kent, D.
AU - Okulov, I. V.
AU - Wendrock, H.
AU - Bönisch, Matthias
AU - Volegov, A. S.
AU - Calin, Mariana
AU - Eckert, Jürgen
AU - Dargusch, M.S.
PY - 2017/3
Y1 - 2017/3
M3 - Article
VL - 688
SP - 20
EP - 26
JO - Materials science and engineering: A, Structural materials: properties, microstructure and processing
JF - Materials science and engineering: A, Structural materials: properties, microstructure and processing
SN - 0921-5093
ER -