Influence of starting temperature on differential scanning calorimetry measurements of an Al–Mg–Si alloy
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Standard
Influence of starting temperature on differential scanning calorimetry measurements of an Al–Mg–Si alloy. / Pogatscher, Stefan; Antrekowitsch, Helmut; Uggowitzer, P.J.
in: Materials letters, Jahrgang 100, 2013, S. 163-165.
in: Materials letters, Jahrgang 100, 2013, S. 163-165.
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Harvard
Pogatscher, S, Antrekowitsch, H & Uggowitzer, PJ 2013, 'Influence of starting temperature on differential scanning calorimetry measurements of an Al–Mg–Si alloy', Materials letters, Jg. 100, S. 163-165.
APA
Pogatscher, S., Antrekowitsch, H., & Uggowitzer, P. J. (2013). Influence of starting temperature on differential scanning calorimetry measurements of an Al–Mg–Si alloy. Materials letters, 100, 163-165.
Vancouver
Pogatscher S, Antrekowitsch H, Uggowitzer PJ. Influence of starting temperature on differential scanning calorimetry measurements of an Al–Mg–Si alloy. Materials letters. 2013;100:163-165.
Author
Bibtex - Download
@article{a894eb9eefda46b394cbd451d56c1787,
title = "Influence of starting temperature on differential scanning calorimetry measurements of an Al–Mg–Si alloy",
author = "Stefan Pogatscher and Helmut Antrekowitsch and P.J. Uggowitzer",
year = "2013",
language = "Deutsch",
volume = "100",
pages = "163--165",
journal = "Materials letters",
issn = "0167-577X",
publisher = "Elsevier",
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Influence of starting temperature on differential scanning calorimetry measurements of an Al–Mg–Si alloy
AU - Pogatscher, Stefan
AU - Antrekowitsch, Helmut
AU - Uggowitzer, P.J.
PY - 2013
Y1 - 2013
M3 - Artikel
VL - 100
SP - 163
EP - 165
JO - Materials letters
JF - Materials letters
SN - 0167-577X
ER -