Influence of modulus-to-hardness ratio and harmonic parameters on continuous stiffness measurement during nanoindentation
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Standard
Influence of modulus-to-hardness ratio and harmonic parameters on continuous stiffness measurement during nanoindentation. / Merle, Benoit; Maier-Kiener, Verena; Pharr, George M.
in: Acta materialia, Jahrgang 134, 2017, S. 167-176.
in: Acta materialia, Jahrgang 134, 2017, S. 167-176.
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Harvard
Merle, B, Maier-Kiener, V & Pharr, GM 2017, 'Influence of modulus-to-hardness ratio and harmonic parameters on continuous stiffness measurement during nanoindentation', Acta materialia, Jg. 134, S. 167-176. https://doi.org/10.1016/j.actamat.2017.05.036
APA
Merle, B., Maier-Kiener, V., & Pharr, G. M. (2017). Influence of modulus-to-hardness ratio and harmonic parameters on continuous stiffness measurement during nanoindentation. Acta materialia, 134, 167-176. https://doi.org/10.1016/j.actamat.2017.05.036
Vancouver
Merle B, Maier-Kiener V, Pharr GM. Influence of modulus-to-hardness ratio and harmonic parameters on continuous stiffness measurement during nanoindentation. Acta materialia. 2017;134:167-176. doi: http://dx.doi.org/10.1016/j.actamat.2017.05.036
Author
Bibtex - Download
@article{63ec50e97dae4baf8b4fbd2926f9d198,
title = "Influence of modulus-to-hardness ratio and harmonic parameters on continuous stiffness measurement during nanoindentation",
author = "Benoit Merle and Verena Maier-Kiener and Pharr, {George M.}",
year = "2017",
doi = "http://dx.doi.org/10.1016/j.actamat.2017.05.036",
language = "English",
volume = "134",
pages = "167--176",
journal = "Acta materialia",
issn = "1359-6454",
publisher = "Elsevier",
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Influence of modulus-to-hardness ratio and harmonic parameters on continuous stiffness measurement during nanoindentation
AU - Merle, Benoit
AU - Maier-Kiener, Verena
AU - Pharr, George M.
PY - 2017
Y1 - 2017
U2 - http://dx.doi.org/10.1016/j.actamat.2017.05.036
DO - http://dx.doi.org/10.1016/j.actamat.2017.05.036
M3 - Article
VL - 134
SP - 167
EP - 176
JO - Acta materialia
JF - Acta materialia
SN - 1359-6454
ER -