Characterization of bulk metallic glasses via fast differential scanning calorimetry

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Standard

Characterization of bulk metallic glasses via fast differential scanning calorimetry. / Pogatscher, Stefan; Leutenegger, D.; Hagmann, A et al.
in: Thermochimica Acta, Jahrgang 590, 2014, S. 84-90.

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Harvard

Pogatscher, S, Leutenegger, D, Hagmann, A, Uggowitzer, PJ & Löffler, JF 2014, 'Characterization of bulk metallic glasses via fast differential scanning calorimetry', Thermochimica Acta, Jg. 590, S. 84-90.

APA

Pogatscher, S., Leutenegger, D., Hagmann, A., Uggowitzer, P. J., & Löffler, J. F. (2014). Characterization of bulk metallic glasses via fast differential scanning calorimetry. Thermochimica Acta, 590, 84-90.

Vancouver

Author

Bibtex - Download

@article{c66a49d1586e45f58a1873f624bdb944,
title = "Characterization of bulk metallic glasses via fast differential scanning calorimetry",
author = "Stefan Pogatscher and D. Leutenegger and A Hagmann and Uggowitzer, {Peter J.} and J.F. L{\"o}ffler",
year = "2014",
language = "Deutsch",
volume = "590",
pages = "84--90",
journal = "Thermochimica Acta",
issn = "0040-6031",
publisher = "Elsevier",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Characterization of bulk metallic glasses via fast differential scanning calorimetry

AU - Pogatscher, Stefan

AU - Leutenegger, D.

AU - Hagmann, A

AU - Uggowitzer, Peter J.

AU - Löffler, J.F.

PY - 2014

Y1 - 2014

M3 - Artikel

VL - 590

SP - 84

EP - 90

JO - Thermochimica Acta

JF - Thermochimica Acta

SN - 0040-6031

ER -