Tuning of material properties of ZnO thin films grown by plasma-enhanced atomic layer deposition at room temperature
Research output: Contribution to journal › Article › Research › peer-review
Authors
Organisational units
External Organisational units
- Graz University of Technology, Institute of Solid State Physics
Details
Original language | English |
---|---|
Article number | 01A109 |
Journal | Journal of Vacuum Science and Technology A: Vacuum, Surfaces and Films |
Volume | 36 |
Issue number | 1 |
DOIs | |