The Precipitation Behavior of Superalloy ATI Allvac 718Plus
Research output: Contribution to journal › Article › Research › peer-review
Standard
The Precipitation Behavior of Superalloy ATI Allvac 718Plus. / Zickler, Gerald; Radis, Rene; Schnitzer, Ronald et al.
In: Advanced Engineering Materials, 2010, p. 176-183.
In: Advanced Engineering Materials, 2010, p. 176-183.
Research output: Contribution to journal › Article › Research › peer-review
Harvard
Zickler, G, Radis, R, Schnitzer, R, Kozeschnik, E, Stockinger, M & Leitner, H 2010, 'The Precipitation Behavior of Superalloy ATI Allvac 718Plus', Advanced Engineering Materials, pp. 176-183. https://doi.org/10.1002/adem.200900282
APA
Zickler, G., Radis, R., Schnitzer, R., Kozeschnik, E., Stockinger, M., & Leitner, H. (2010). The Precipitation Behavior of Superalloy ATI Allvac 718Plus. Advanced Engineering Materials, 176-183. https://doi.org/10.1002/adem.200900282
Vancouver
Zickler G, Radis R, Schnitzer R, Kozeschnik E, Stockinger M, Leitner H. The Precipitation Behavior of Superalloy ATI Allvac 718Plus. Advanced Engineering Materials. 2010;176-183. doi: 10.1002/adem.200900282
Author
Bibtex - Download
@article{e31803c0e7a849dc886751c4f6700245,
title = "The Precipitation Behavior of Superalloy ATI Allvac 718Plus",
author = "Gerald Zickler and Rene Radis and Ronald Schnitzer and Ernst Kozeschnik and Martin Stockinger and Harald Leitner",
year = "2010",
doi = "10.1002/adem.200900282",
language = "English",
pages = "176--183",
journal = "Advanced Engineering Materials",
issn = "1438-1656",
publisher = "Wiley-VCH ",
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - The Precipitation Behavior of Superalloy ATI Allvac 718Plus
AU - Zickler, Gerald
AU - Radis, Rene
AU - Schnitzer, Ronald
AU - Kozeschnik, Ernst
AU - Stockinger, Martin
AU - Leitner, Harald
PY - 2010
Y1 - 2010
U2 - 10.1002/adem.200900282
DO - 10.1002/adem.200900282
M3 - Article
SP - 176
EP - 183
JO - Advanced Engineering Materials
JF - Advanced Engineering Materials
SN - 1438-1656
ER -