Deformation and fracture behaviors of K403 Ni-based superalloy at elevated temperatures

Research output: Contribution to journalArticleResearchpeer-review

Authors

Organisational units

External Organisational units

  • School of Materials Science and Engineering, Xi'an University of Technology

Details

Original languageEnglish
Pages (from-to)581-590
Number of pages10
JournalJournal of alloys and compounds
Volume699.2017
Issue number30 March