A study of the micro- and nanoscale deformation behavior of individual austenitic dendrites in a FeCrMoVC cast alloy using micro- and nanoindentation experiments

Research output: Contribution to journalArticleResearchpeer-review

Authors

  • J. Zeisig
  • J. Hufenbach
  • H. Wendrock
  • T. Gemming
  • U. Kühn

Organisational units

External Organisational units

  • Institute for Complex Materials
  • TU Dresden

Details

Original languageEnglish
Article number143103
JournalApplied physics letters
Volume108
Issue number14
DOIs
Publication statusPublished - 4 Apr 2016