The Precipitation Behavior of Superalloy ATI Allvac 718Plus

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Standard

The Precipitation Behavior of Superalloy ATI Allvac 718Plus. / Zickler, Gerald; Radis, Rene; Schnitzer, Ronald et al.
in: Advanced Engineering Materials, 2010, S. 176-183.

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Vancouver

Zickler G, Radis R, Schnitzer R, Kozeschnik E, Stockinger M, Leitner H. The Precipitation Behavior of Superalloy ATI Allvac 718Plus. Advanced Engineering Materials. 2010;176-183. doi: 10.1002/adem.200900282

Bibtex - Download

@article{e31803c0e7a849dc886751c4f6700245,
title = "The Precipitation Behavior of Superalloy ATI Allvac 718Plus",
author = "Gerald Zickler and Rene Radis and Ronald Schnitzer and Ernst Kozeschnik and Martin Stockinger and Harald Leitner",
year = "2010",
doi = "10.1002/adem.200900282",
language = "English",
pages = "176--183",
journal = "Advanced Engineering Materials",
issn = "1438-1656",
publisher = "Wiley-VCH ",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - The Precipitation Behavior of Superalloy ATI Allvac 718Plus

AU - Zickler, Gerald

AU - Radis, Rene

AU - Schnitzer, Ronald

AU - Kozeschnik, Ernst

AU - Stockinger, Martin

AU - Leitner, Harald

PY - 2010

Y1 - 2010

U2 - 10.1002/adem.200900282

DO - 10.1002/adem.200900282

M3 - Article

SP - 176

EP - 183

JO - Advanced Engineering Materials

JF - Advanced Engineering Materials

SN - 1438-1656

ER -